Coating process and matters needing attention
Release time:
2020-11-10 13:44
Source:
One. Application of Pre-Primer
1. Before spraying, the substrate must be treated to be free of rust and oil, and kept clean and dry.
2. If the product is a two-component system, first stir the paint slurry evenly, add the curing agent in proportion, stir and mature for 30 minutes.
3. Adjust the construction viscosity with special diluent, and match the paint according to the dosage. The paint should be used up within 8 hours.
4. It is recommended to spray 1, the viscosity is 15-18 seconds (coating -4#), and the maximum dry film thickness is 25μm
II. Application of Primer
1. Before coating, the substrate must be treated to be free of rust and oil, and kept clean and dry.
2. The product is a two-component system. First, stir the lacquer slurry evenly, add the curing agent in proportion, stir and mature for 30 minutes.
3. Special diluent to adjust the construction viscosity, according to the amount of paint, with a good paint should be used up within 8 hours
4. It is recommended to spray 2, the viscosity is 15-18 seconds (coating -4#), and the maximum thickness of each dry film is 355μm. The construction interval is more than 20 minutes
5. If you need to polish in the environment above 15 ℃, dry for 24 hours
Three. Construction of unsaturated polyester putty
1. After the bottom gas is completely dry, you can carry out the construction of putty
2. After opening the barrel cover, stir the putty in the barrel evenly, and add the curing agent according to the proportion to mix evenly, then the scraping construction can be carried out
3. First scrape a 15# putty, then scrape two 11# putty, then use three 15# putty
4. After scraping each putty for 4 hours, polish it, then scrape off another putty, and the last one needs to be carefully polished. If the winter temperature is low, need to extend the grinding time or add catalyst, adjust the curing time
5. The putty should be used up within 10-30 minutes. According to the construction needs, the application time can also be adjusted by adjusting the dosage of curing agent.
Four. Application of Intermediate Primer
1. After scraping the putty and polishing it flat, you can spray the primer
2. Stir the paint slurry in the barrel evenly, add the curing agent according to the proportion, and mature for 30 minutes.
3. According to the amount of paint, paint should be used up in 8 hours
4. with special diluent deployment to the construction viscosity (about -4# cup, 17-22 seconds) can be air spraying
5. It is recommended to spray two coats at an interval of 24 hours, and after the second coat is completely dry (the ambient temperature is above 15 ℃ for 24 hours, according to the construction needs, fill the defects with putty, polish with sandpaper, and then spray the second coat primer)
6. It is required that the undercoat film shall be smooth and free of sagging.
Five. Construction of topcoat
1. The substrate is required to be dry without water beads, oil stains and other impurities.
2. After 24 hours of drying of the paint in the second pass. Finish construction can be carried out
3. According to the amount of paint, paint should be used up within 8 hours
4. Open the lid of the barrel, fully stir the paint slurry in the barrel, add the curing agent according to the proportion, stir well and place it for 20 minutes before use
5. The use of supporting special supporting diluent for thinning, spraying viscosity is about 17-23 seconds
6. Spray a top coat first to find and repair the defects of the substrate. After the defects are treated, spray the next coat. Each coat must be dried at an environment above 15 ℃ for 2 hours, and then spray the next coat. If color matching is carried out, it must be dried for 24 hours.
7. If you need to polish, you must let the paint film dry at room temperature for 18 hours before dipping in water
The spraying process requires harsh environmental conditions, and natural conditions have many inconveniences. Such as air flow, air humidity, temperature changes. recommend use Polaroid RP-1 water-based paint hair dryer, and RPS-1 stand-up blow gun holder.
Next Page
More Solutions
General technical essentials for spraying with a spray gun
2020-11-10
1. the general essentials of using spray gun for repair spraying technology: 1) Hold the gun. The gun is held by the palm, thumb, little finger and ring finger, and the middle and index fingers are used to pull the trigger. Some painters change the way they hold the gun from time to time when they work for a long time. Sometimes they only use their thumb and palm to cooperate with their little finger, sometimes they use their ring finger to hold the gun. The middle finger and index finger are used to pull the trigger. This can relieve fatigue and improve labor efficiency. 2. The orientation of the spray gun to the surface of the substrate. The spray gun should be kept perpendicular to the surface of the substrate, or as vertical as possible. If the spray gun is a little skewed, the result will inevitably cause the spray band to flow on one side, while the other side appears dry and thin, lacking paint, which is very likely to cause striped coating. 3. Distance from spray gun to substrate surface. For the siphon spray gun, the best working distance is 15~20cm. If the distance is too close, it may produce runny, and may even cause color inconsistency with expectations when spraying metallic flash paint or pearl paint. If the distance is too far. More than 20cm, it may lead to dry spray, overspray, so that the leveling of the coating is poor. If metallic glitter paint is sprayed, there may also be the possibility of color change. The press-fed spray gun can be farther away from the substrate. Generally, the best distance is about 20~30cm. These are the basic principles that must be followed when spraying construction. 4. The moving speed of the spray gun. When spraying, the moving speed of the spray gun has a great influence on the coating effect. If the spray gun moves too fast, the surface appears dry and thin, poor leveling and rough; if the spray gun moves too slowly, the formed coating is too thick, and it is very likely to cause sagging. The most ideal spray gun moving speed should be once the spray is over, the new spray layer looks so plump, wet, neither dry, barren, nor excessively piled up. In short, the moving speed of the spray gun should be determined according to the specific conditions of the construction site. Generally speaking, only for relative comparison, the movement speed of the press type spray gun is faster than that of other types of spray guns. 5. Trigger control. The gun is controlled by the trigger. The deeper the trigger is pulled, the greater the liquid flow rate. In the process of traditional gun walking, the trigger is always pressed, not half-pressed. In order to avoid the accumulation of paint sprayed at the end of each gun walk, experienced painters should relax the trigger slightly to reduce the amount of paint supplied.
Coating process and matters needing attention
2020-11-10
One. Application of Pre-Primer 1. Before spraying, the substrate must be treated to be free of rust and oil, and kept clean and dry. 2. If the product is a two-component system, first stir the paint slurry evenly, add the curing agent in proportion, stir and mature for 30 minutes. 3. Adjust the construction viscosity with special diluent, and match the paint according to the dosage. The paint should be used up within 8 hours. 4. It is recommended to spray 1, the viscosity is 15-18 seconds (coating -4#), and the maximum dry film thickness is 25μm II. Application of Primer 1. Before coating, the substrate must be treated to be free of rust and oil, and kept clean and dry. 2. The product is a two-component system. First, stir the lacquer slurry evenly, add the curing agent in proportion, stir and mature for 30 minutes. 3. Special diluent to adjust the construction viscosity, according to the amount of paint, with a good paint should be used up within 8 hours 4. It is recommended to spray 2, the viscosity is 15-18 seconds (coating -4#), and the maximum thickness of each dry film is 355μm. The construction interval is more than 20 minutes 5. If you need to polish in the environment above 15 ℃, dry for 24 hours Three. Construction of unsaturated polyester putty 1. After the bottom gas is completely dry, you can carry out the construction of putty 2. After opening the barrel cover, stir the putty in the barrel evenly, and add the curing agent according to the proportion to mix evenly, then the scraping construction can be carried out 3. First scrape a 15# putty, then scrape two 11# putty, then use three 15# putty 4. After scraping each putty for 4 hours, polish it, then scrape off another putty, and the last one needs to be carefully polished. If the winter temperature is low, need to extend the grinding time or add catalyst, adjust the curing time 5. The putty should be used up within 10-30 minutes. According to the construction needs, the application time can also be adjusted by adjusting the dosage of curing agent. Four. Application of Intermediate Primer 1. After scraping the putty and polishing it flat, you can spray the primer 2. Stir the paint slurry in the barrel evenly, add the curing agent according to the proportion, and mature for 30 minutes. 3. According to the amount of paint, paint should be used up in 8 hours 4. with special diluent deployment to the construction viscosity (about -4# cup, 17-22 seconds) can be air spraying 5. It is recommended to spray two coats at an interval of 24 hours, and after the second coat is completely dry (the ambient temperature is above 15 ℃ for 24 hours, according to the construction needs, fill the defects with putty, polish with sandpaper, and then spray the second coat primer) 6. It is required that the undercoat film shall be smooth and free of sagging. Five. Construction of topcoat 1. The substrate is required to be dry without water beads, oil stains and other impurities. 2. After 24 hours of drying of the paint in the second pass. Finish construction can be carried out 3. According to the amount of paint, paint should be used up within 8 hours 4. Open the lid of the barrel, fully stir the paint slurry in the barrel, add the curing agent according to the proportion, stir well and place it for 20 minutes before use 5. The use of supporting special supporting diluent for thinning, spraying viscosity is about 17-23 seconds 6. Spray a top coat first to find and repair the defects of the substrate. After the defects are treated, spray the next coat. Each coat must be dried at an environment above 15 ℃ for 2 hours, and then spray the next coat. If color matching is carried out, it must be dried for 24 hours. 7. If you need to polish, you must let the paint film dry at room temperature for 18 hours before dipping in water The spraying process requires harsh environmental conditions, and natural conditions have many inconveniences. Such as air flow, air humidity, temperature changes. recommend use Polaroid RP-1 water-based paint hair dryer, and RPS-1 stand-up blow gun holder.
Pretreatment of spraying process
2020-11-10
The whole process of spraying process mainly includes four parts: pre-coating process, small parts coating process, large structural parts coating process and whole machine coating process. Among them, the coating process of small parts is the most important process in the production process of the product, and it is the main protective work carried out by the parts before coating and before assembly. The process flow includes pre-coating treatment, drying, primer spraying, leveling, topcoat spraying, leveling, drying and other processes.
The correct method of selecting the paint-saving environmental protection spraying equipment.
2020-11-10
The transmission efficiency of the traditional air spray gun (I. e. paint utilization rate) is about 30%, while the other 70% or so of the spraying solvent is scattered into the surrounding environment with the flying fog, wasting a large amount of paint or coating, which not only increases the economic cost, but also emits very large amounts of toxic and harmful substances such as TVOC, benzene and formaldehyde, seriously polluting the atmosphere and water environment, and damaging the health of the builders. The use of HVLP standard spray gun or spraying equipment, can greatly reduce the fog and rebound (spray), reduce paint, photocatalyst and other solvent emissions, greatly save the amount of spraying, while keeping the working environment clean, protect the atmospheric environment and construction personnel health.
WeChat Public Number
COPYRIGHT©2023 Guangzhou Baoli Air Tools Co., Ltd. ALL RIGHTS RESERVED.Powered by www.300.cn SEO Tags Business License